(5 pc) 1/4" Drive Titanium & Superalloy Socket Set 6-Pt (PREORDER)
(5 pc) 1/4" Drive Titanium & Superalloy Socket Set 6-Pt (PREORDER)
(5 pc) 1/4" Drive Titanium & Superalloy Socket Set 6-Pt (PREORDER)
(5 pc) 1/4" Drive Titanium & Superalloy Socket Set 6-Pt (PREORDER)
  • ギャラリービューアに画像を読み込む{{ imageAlt </ p5>
  • ギャラリービューアに画像を読み込む{{ imageAlt </ p5>
  • ギャラリービューアに画像を読み込む{{ imageAlt </ p5>
  • ギャラリービューアに画像を読み込む{{ imageAlt </ p5>

(5 pc) 1/4" Drive Titanium & Superalloy Socket Set 6-Pt (PREORDER)

通常価格
完売
セールスプライス
$215.00

The most Premium Socket Set on the market. 

The lightest, tightest fitting sockets using the best materials and coatings.

ESTIMATED SHIP DATE: LATE JULY 2025

THE PRODUCT IMAGES ARE RENDERS OF THE FINAL PRODUCT DESIGN THAT IS IN PRODUCTION.
SURFACE FINISH AND MARKINGS WILL BE SIMILAR TO (OR BETTER THAN) OUR SPARK PLUG SOCKETS SHOWN BELOW.

Features of the TRO Titanium & Superalloy Socket Set:

  • 6, 8, 10 & 12 mm sockets, beautifully machined from Titanium Ti-6AL-4V (Grade 5). High quality surface finish inside and out.

  • 1/4" Hex Bit Holder machined from one of the strongest metals on Earth.
    This "Superalloy" combined w/ extremely tight clearance fitment allows for the Ultimate in Ultralight design. 

  • Our Superalloy material conforms to Mil-Spec, DFARS, Aerospace Material Specifications (AMS) and (3) GE Aviation Standards. Vacuum Induction Melted (VIM) followed by Vacuum Arc Remelting (VAR) ensures minimal impurities = exceptional fracture toughness.



  • Ultra-lightweight at 27 g (0.95 oz) total. Half the mass of an equivalent normal socket set - there's no better set for a lightweight toolkit.

  • Exceptionally tight clearances. Both Hexes and the square drive offer much better fitment than standard tools. A near perfect fit on fasteners and hex bits.

  • With minimal play between the socket and fastener, more of the socket is engaged, reducing stress on the tool.


                     
  • Extremely strong retention design on the 1/4" square drive.

  • Several high performance PVD Coatings Offered:

     

    COATING SURFACE
    HARDNESS (VICKERS)
    THICKNESS (μm) FRICTION
    COEF.
    UNCOATED TITANIUM 400 0.4
    UNCOATED SUPERALLOY 550 -
    CHROME PLATING (FOR COMPARISON) 950 20-40 0.2
    DLC (CHARCOAL) 1600 3 0.1-0.2
    TiN (GOLD) 3000 3 0.6
    CrN (DARK IRIDESCENT) 3000 7 0.5
    AlCrN (BLUE-GRAY) 4490 5 0.35

    Coating Color Examples:

    Dark Iridescent Chromium Nitride (Sunset):
    (this coating may vary in color)


    TRO Dark Iridescent Chromium Nitride Coating
Blue-Gray AlCrN 44 GPa:

TRO_Blue_Gray_AlCrN_Coating


Customer Reviews

Based on 1 review
100%
(1)
0%
(0)
0%
(0)
0%
(0)
0%
(0)
C
C.S. Garcia
5 piece socket set

Amazing set!! All the most common sizes for Motorbikes but you’d be surprised how common those sizes are for most other applications!! Super precise fitting, zero wobble, and the finishes offered are unlike most other manufacturer out there. I went with the AlCrNfinish for the sockets and TiN for a spare 10mm that I hope I never need ;) . LOOKING FORWARD TO FUTURE PROJECTS!!