The most Premium Bit Holder Socket on the market. 

The lightest, tightest fitting socket using the best materials and coatings.

Features of the TRO Superalloy Bit Holder Socket:

  • 1/4" Hex Bit Holder machined from one of the strongest metals on Earth.
    This "Superalloy" combined w/ extremely tight clearance fitment allows for the Ultimate in Ultralight design. 

  • Our Superalloy material conforms to Mil-Spec, DFARS, Aerospace Material Specifications (AMS) and (3) GE Aviation Standards. Vacuum Induction Melted (VIM) followed by Vacuum Arc Remelting (VAR) ensures minimal impurities = exceptional fracture toughness.



  • Ultra-lightweight at 8.1 g (0.28 oz) total; 31-38% Lighter than other premium, slim design bit holders. 


  • Exceptionally tight clearances. Both Hexes and the square drive offer much better fitment than standard tools. A near perfect fit on fasteners and hex bits.

  • With minimal play between the socket and fastener, more of the socket is engaged, reducing stress on the tool.


                     
  • Extremely strong retention design on the 1/4" square drive.

  • Several high performance PVD Coatings Offered:

     

    COATING SURFACE
    HARDNESS (VICKERS)
    THICKNESS (μm) FRICTION
    COEF.
    UNCOATED TITANIUM 400 0.4
    UNCOATED SUPERALLOY 550 -
    CHROME PLATING (FOR COMPARISON) 950 20-40 0.2
    DLC (CHARCOAL) 1600 3 0.1-0.2
    TiN (GOLD) 3000 3 0.6
    CrN (DARK IRIDESCENT) 3000 7 0.5
    AlCrN (BLUE-GRAY) 4490 5 0.35

    Coating Color Examples: